Soluble Salts beneath Coatings - An Overview

From JPCL, February 2010

More items for Quality Control; Surface Preparation

by Kenneth B. Tator, P.E., KTA-Tator, Inc.

Part 1 in a series on soluble salts, this article offers a summary of recent research on allowable amounts of salts tolerated beneath coatings....
(Login to read the full article)

   

Tagged categories: Exposure conditions; Exterior industrial pollutant exposure; Flash rusting; Immersion service; Salt contaminant levels; Salt exposure; Soluble salts; Surface preparation

Comment Join the Conversation:

Sign in to our community to add your comments.

Fischer Technology Inc.
DUALSCOPE® MP0R Coating Thickness Gauge

• Meets requirements of corrosion and painting industry; Ideal for SSPC-PA2, IMO PSPC
• Use w/ Ferrous and Non-Ferrous substrates
• Two backlit displays
Call 800-243-8417


Atlantic Design, Inc.
It’s All True!

We custom design equipment; We upgrade existing equipment; We rent equipment; We have the best service in the industry. WE REALLY DO KNOW EQUIPMENT! 866.Call.ADI


DeFelsko Corporation
NEW PosiTector
Inspection Kits

PosiTector 6000 Coating Thickness Gage easily converts to a surface profile gage, dew point meter or ultrasonic wall thickness gage with a simple probe change.


Axxiom Manufacturing
Schmidt Improves
Portable Blasters

Schmidt's VBS System reduces blowdown intensity, prevents exhaust from damaging floor while using no screens or filters. Reduces sound; Increasing safety.
Call 1-800-231-2085


Van Air Systems
Moisture problems in your air lines?

Van Air Systems' Blast Pak is a portable compressed air drying system that reduces downtime in all blasting and coating applications.


Novatek Corporation
Dustless Coatings Removal

Strip it, clean it, and profile it,
all dust free! High production
rates and Blast like finishes.
Comply with new lead
standards.


International Paint LLC
Our New Protective Coatings Centers

Our complete range of International and Devoe Coatings products are available at our Protective Coatings Centers, making purchases faster and easier.

 
 
 
 
Technology Publishing

The Technology Publishing Network

The Journal of Protective Coatings & Linings (JPCL) PaintSquare
Durability + Design Paint BidTracker JPCL Europe

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy policy   |   Terms & conditions   |   Site Map   |   Search   |   Contact Us
 

© Copyright 2000-2013, Technology Publishing / PaintSquare, All rights reserved
2100 Wharton Street, Suite 310, Pittsburgh PA 15203-1951; Tel 1-412-431-8300; Fax 1-412-431-5428; E-mail webmaster@paintsquare.com