Preventing Coating Damage in the Supply Chain of Pipelines

From JPCL, February 2010

More items for Program/Project Management; Quality Control

by Idsart van Assema, Line Pipe Logistic Innovation & Research Center

The author describes in-house employee observations as well as literature on coating damage in the field during incorrect handling, storage, and transport of pipes. Root causes and ways to prevent it are also discussed, including the use of special handling and storage equipment....
(Login to read the full article)

   

Tagged categories: Abrasion; Coating failure; Pipelines; UV resistance

Comment Join the Conversation:

Sign in to our community to add your comments.

DeFelsko Corporation
NEW PosiTector
Inspection Kits

PosiTector 6000 Coating Thickness Gage easily converts to a surface profile gage, dew point meter or ultrasonic wall thickness gage with a simple probe change.


Fischer Technology Inc.
Gauges Meet IMO-PSPC & SSPC-PA2 Requirements

• USB or optional Bluetooth
• Custom inspection reports
• Excellent on edges & rough surfaces; Optimum accuracy
• Largest selection of probes to meet challenging situations
Call Fischer: 800-243-8417


Bayer MaterialScience LLC
Desmodur® XP 2763 Drives Financial Results

High performance polyaspartic coatings
• Dry faster
• Fewer coats
• Superior corrosion/weather resistance
412-777-3983


SAFE Systems, Inc.
Enduroguard -
The Tough Cable
for a Tough Industry.

Reduce maintenance costs and down time, increase job site safety with Enduroguard Cable. Available exclusively from SAFE Systems. UL listed, flexible, abrasion resistant and cut resistant.


Polyval Coatings
POLYFLEX brand Polyurea

high chemical resistant membranes are used extensively to protect our environment in secondary containment applications.


ElektroPhysik
High-precision coating thickness gauge MiniTest 7400

MiniTest 7400 with intuitive menu control, enhanced data management with configuration assistent. Wear-resistant sensors for measuring tasks up to 35mm thickness.


Denso North America Inc.
Denso SeaShield
Marine Systems

A full range of steel, concrete and timber pile rehabilitation systems including petrolatum systems, fiberglass jackets, epoxy grouts and many other product lines.
Call 1-281-821-3355 or Visit densona.com

 
 
 
 
Technology Publishing

The Technology Publishing Network

The Journal of Protective Coatings & Linings (JPCL) PaintSquare
Durability + Design Paint BidTracker JPCL Europe

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy policy   |   Terms & conditions   |   Site Map   |   Search   |   Contact Us
 

© Copyright 2000-2013, Technology Publishing / PaintSquare, All rights reserved
2100 Wharton Street, Suite 310, Pittsburgh PA 15203-1951; Tel 1-412-431-8300; Fax 1-412-431-5428; E-mail webmaster@paintsquare.com