Investigating Corrosion Protection of Offshore Wind Towers, Part 3: Results of the Laboratory Investigations

From JPCL, November 2009

More items for Coating Materials

by Andreas W. Momber, Ph.D., Muehlhan AG; Peter Plagemann, Ph.D., and Volkmar Stenzel, Ph.D., Fraunhofer Institute for Manufacturing and Applied Materials Research; and Michael Schneider, Ph.D., Fraunhofer Institute for Ceramic Technologies and Systems

In Part 3 of a three-part series, the authors report on corrosive stress on offshore wind towers. Laboratory investigations of several coatings for wind towers are discussed and compared with site testing of the same coatings....
(Login to read the full article)

   

Tagged categories: Accelerated laboratory testing; Cathodic protection; Corrosion protection; Electrical Impedance; Epoxy; Laboratory testing; Offshore; Polyurethane; Site/field testing; Wind Towers

Comment Join the Conversation:

Sign in to our community to add your comments.

BASF
New resins from BASF will have metals loving water:

Excellent corrosion resistance, low VOC, high gloss, thin films basf.us/industrialcoatings
polyorders@basf.com
800-231-7868


Versaflex Inc.
Best NSF 61.5 Approved Potable Water Polyurea

VersaFlex Polyurea Earns Highest ANSI/NSF 61.5 Rating for High Temp Service, Minimum Tank Size and Max Thickness. All Polyureas Are Not Created Equal. FREE WHITE PAPER.


Sherwin-Williams
Ask Sherwin-Williams

Does your Paint company know where your Paint is?
If your paint company is Sherwin-Williams it does.
Leave Nothing to Chance


Wasser High-Tech Coatings Inc.
Wasser Coatings

have been used to protect some of the most important bridges in the country; learn about our NEPCOAT-approved system as well as our entire range of MCU coatings and Polyurea membranes.


Denso North America Inc.
Tank Base Protection

An easy to apply system utilizing Denso tapes and coatings around the tank base, that helps prevent corrosion from external elements.
Call 1-281-821-3355 or Visit densona.com


Dow Corning Corporation
New Dow Corning® 3055 Resin

Ensure long-term asset protection and extend repaint cycles with a low-VOC, two-coat polysiloxane coating featuring superior corrosion and moisture resistance.


Bayer MaterialScience LLC
Desmodur® XP 2763 Drives Financial Results

High performance polyaspartic coatings
• Dry faster
• Fewer coats
• Superior corrosion/weather resistance
412-777-3983

 
 
 
 
Technology Publishing

The Technology Publishing Network

The Journal of Protective Coatings & Linings (JPCL) PaintSquare
Durability + Design Paint BidTracker JPCL Europe

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy policy   |   Terms & conditions   |   Site Map   |   Search   |   Contact Us
 

© Copyright 2000-2013, Technology Publishing / PaintSquare, All rights reserved
2100 Wharton Street, Suite 310, Pittsburgh PA 15203-1951; Tel 1-412-431-8300; Fax 1-412-431-5428; E-mail webmaster@paintsquare.com