Selecting and Sourcing Coatings for Transmission Pipelines

Coating Sheet Pile Structures: An Overview

From JPCL, April 2009

by Timothy Race, Kaked LLC

This article gives an overview of steel piling and its uses; reasons for coating it; shop coating of new steel piling; and ways to access, inspect, and perform maintenance coating of installed steel piling....
(Login to read the full article)

   

Tagged categories: Coal tar epoxy; Corrosion protection; Epoxy; Fusion bonded epoxy; Polyurethane; Steel pilings

Comment Join the Conversation:

Sign in to our community to add your comments.

Denso North America Inc.
Tank Base Protection

An easy to apply system utilizing Denso tapes and coatings around the tank base, that helps prevent corrosion from external elements.
Call 1-281-821-3355 or Visit densona.com


Dow Corning Corporation
New Dow Corning® 3055 Resin

Ensure long-term asset protection and extend repaint cycles with a low-VOC, two-coat polysiloxane coating featuring superior corrosion and moisture resistance.


Bayer MaterialScience LLC
Desmodur® XP 2763 Drives Financial Results

High performance polyaspartic coatings
• Dry faster
• Fewer coats
• Superior corrosion/weather resistance
412-777-3983


Rapid Prep, LLC
Nation Wide Equipment Rentals

Rapid Prep, LLC is a full service provider of sandblasting & all other surface preparation equipment, with 60 years of experience within the industrial painting industry.


NLB Corporation
Handheld VertaJet™ for concrete or steel

Ergonomic VertaJet from NLB boosts surface prep productivity. Rotating 40,000 psi water jets strip a 6” path and get into corners, with vacuum recovery.


Hempel (USA) Inc.
Real Coating
for Real Protection

Hempel's protective coatings cover a wide range of applications across multiple industries from oil and gas to power generation to infrastructure.


JPCL - PCE - PaintSquare
Charter Advertising Opportunities Available through April 30.

Click above or contact Bernadette Landon
Publisher, JPCL Europe blandon@jpcleurope.com +1.412.697.0184
visit www.jpcleurope.com

 
 
 
 
Technology Publishing

The Technology Publishing Network

The Journal of Protective Coatings & Linings (JPCL) PaintSquare
Durability + Design Paint BidTracker JPCL Europe

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy policy   |   Terms & conditions   |   Site Map   |   Search   |   Contact Us
 

© Copyright 2000-2013, Technology Publishing / PaintSquare, All rights reserved
2100 Wharton Street, Suite 310, Pittsburgh PA 15203-1951; Tel 1-412-431-8300; Fax 1-412-431-5428; E-mail webmaster@paintsquare.com