A Methodology to Evaluate the Relative Performance of Various Coating Systems

From JPCL, March 2009

by Shuang-Ling Chong, Federal Highway Administration (retired 2007), and Yuan Yao, SES Group & Associates

This article discusses the various accelerated laboratory test methods that have been developed to predict a coating's field performance in a relatively short time....
(Login to read the full article)

   

Tagged categories: Aluminum pigment; Bridges; Laboratory testing; MIO; Performance testing; Urethane; Zinc-rich (inorganic); Zinc-rich (organic)

Comment Join the Conversation:

Sign in to our community to add your comments.

Advertisements
 
SAFE Systems, Inc.
 
Custom blast rooms
by SAFE Systems
 
Don't waste time and money "making do" with a "standard" design. Let us work with you to design and build the system that best fits your requirements.
Call 1-800-634-7278
 

 
Detail Masters
 
Overspray Removal
 
We offer professional, turnkey service and unparalleled quality!
Our process can save hundreds— even thousands of dollars. It's fast, environmentally safe and 100% guaranteed.
 

 
Industrial Vacuum Equipment Corp.
 
Hurricane Vacuums
& Dust Collectors
 
Vacuum and dust collector hose, filters and related accessories.
IndustrialVacuum.com
 

 
SABRE Autonomous Solutions
 
Repeatability
 
The ALPHA1 provides reliable results consistently allowing you to cost your next job with confidence.
 

 
HoldTight Solutions Inc.
 
NO FLASH RUST - NO CONTAMINANTS
 
Our HoldTight®102 salt remover & flash rust
preventer prevents flash
rust by removing surface contaminants. Contact us
for your nearest distributor.
(800) 319.8802 sales@holdtight.com
 

 
KTA-Tator, Inc. - Corporate Office
 
KTA-TATOR LABORATORY SERVICES
 
• Coating failure analysis
• Independent testing
• Accelerated weathering testing
• Abrasives Testing
• Oil & Gas Material Qualification
• A2LA Certificate #2455.01
Contact: Rob Leggat
at 412-788-1300 x176
 

 
Graco Inc.
 
Graco EcoQuip 2: Experience the Difference
 
While others claim their equipment is the same, none of them compare to Graco’s EcoQuip 2™ Vapor Abrasive® blasting line. Visit graco.com/ecoquip to learn more.
 

 
Sauereisen, Inc.
 
SewerGard® 210XHB
 
• 300 mils in a single coat by plural component equipment
• Fast Setting
• 100% Solids Epoxy
• Chemical-resistant barrier for municipal wastewater environments
sauereisen.com
 

 
Fischer Technology Inc.
 
DUALSCOPE®FMP100 with DataCenter IP
 
Transfer customized inspection plans from PC to FMP100 using step-by-step guidance with prompts and pictures throughout the measurement procedure
 

 
Modern Safety Techniques
 
Modern Safety Techniques
 
With our unique LTCat, we can help to provide clean, safe breathing air to your workers. Take a look at our Breathing Air Systems, we supply at least twice as much charcoal as our competitors! Modern
 

 
 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

Durability + Design PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy policy (Updated 1/8/2018)   |   Terms & conditions   |   Site Map   |   Search   |   Contact Us