Improving Polyurethane Pipe Coatings for Harsh Conditions

From JPCL, August 2014

More items for Coating Materials

By Andreas aus der Wieschen, Matthias Wintermantel, Todd Williams and Ahren Olson, Bayer MaterialScience AG

This article describes polyurethane pipe coatings as a versatile product class that can be tailored to meet a wide range of end-use applications by varying the formulation....


(Login to read the full article)

   

Tagged categories: Bayer MaterialScience; Formulating; High-performance coatings; Performance testing; Pipeline; Polyurea; Site/field testing

Comment Join the Conversation:

Sign in to our community to add your comments.

Advertisements
 
Mitsubishi Gas Chemical America
 
Performance Amine 1,3-BAC
 
A highly reactive cycloaliphatic diamine offering superior performance. Reasonable cost and curing efficacy makes it suitable for all types of epoxy resin applications.
 

 
Carboline Company
 
New product: Carbozinc® 608 HB
 
Introducing a new high build zinc-rich primer that can save you time and money by eliminating the epoxy intermediate coat!
 

 
Novatek Corporation
 
Dustless Coatings Removal
 
Novatek Corporation, Dustless Coatings Removal Strip, clean and profile all dust free! Comply with new lead standards. Contact today: (866) 563-7800 www.Novatekco.com
 

 
SAFE Systems, Inc.
 
Portable Dust Collectors for Tough Environments
 
Trailer and skid-mounted models in numerous sizes, powered by electric and/or diesel. Sloped roofs, multiple dust inlets, high static, dampered fans. Lockable power & drive compartments.
 

 
BASF
 
New resins from BASF will have metals loving water!
 
Excellent corrosion resistance, low VOC, high gloss, thin films www.basf.us/industrialcoatings dpsolutions@basf.com 800-231-7868
 

 
Jotun Paints Inc.
 
Jotun Jotachar 1709
 
Mesh-free passive fire protection epoxy designed to protect against hydrocarbon pool fire scenarios for up to four hours as defined in the ANSI/UL1709 standard.
 

 
Absolute Equipment/Grand Rental Station
 
TIER 4 EQUIPMENT
 
We have Tier 4 Equipment including Air Compressors & Generators for Sale & Rent! Your job may now require Tier-4. www.absoluteequip.com or Call 412-931-6655.
 

 
SABRE Autonomous Solutions
 
Quality
 
The ALPHA1 provides a consistent finish day-in
day-out; job to job.
 

 
ARC / A.W. Chesterton Company
 
HT-S
 
ARC HT-S is a 100% solids glass/ceramic reinforced novolac epoxy lining for high temperature aqueous cold wall corrosion conditions. ARC HT-S is easily applied by roller, brush, squeegee, or airless spray.
 

 
NLB Corporation
 
NLB Sure Shroud: Greater Protection and Flexibility
 
NLB’s Sure Shroud’s lighter weight and flexibility reduces operator fatigue and offers unmatched protection against high pressure hose ruptures. 10k to 40k psi rated.
 

 
 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

Durability + Design PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us