Preventing and Solving Delamination During Multilayer Pipeline Girth Weld Coating Application

From JPCL, February 2014

More items for Coating Application

by J. Alan Kehr, Alan Kehr Anti-Corrosion, LLC

The author will explain ways to prevent delamination of fusion-bonded epoxy and three-layer polyolefin coating systems in the girth weld areas of newly installed pipelines....
(Login to read the full article)

   

Tagged categories: Adhesion; Coating failure; Corrosion protection; Delamination; Disbondment; Fusion bonded epoxy; Paint application; Pipeline; Polyethylene; Polypropylene

Comment Join the Conversation:

Sign in to our community to add your comments.

Advertisements
 
Industrial Vacuum Equipment Corp.
 
Hurricane Vacuums
& Dust Collectors
 
Vacuum and dust collector hose, filters and related accessories.
IndustrialVacuum.com
 

 
SAFE Systems, Inc.
 
Custom blast rooms
by SAFE Systems
 
Don't waste time and money "making do" with a "standard" design. Let us work with you to design and build the system that best fits your requirements.
Call 1-800-634-7278
 

 
SEMicro Division, M.E. Taylor Engineering, Inc.
 
Coatings Adhesion Testers
 
The PATTI® accurately measures the bond strength between coating & substrate. Outfitted properly, the surface can be rough, porous, or curved & >10K psi strong!
 

 
SABRE Autonomous Solutions
 
Repeatability
 
The ALPHA1 provides reliable results consistently allowing you to cost your next job with confidence.
 

 
Fischer Technology Inc.
 
DUALSCOPE®FMP100 with DataCenter IP
 
Transfer customized inspection plans from PC to FMP100 using step-by-step guidance with prompts and pictures throughout the measurement procedure
 

 
ARC / A.W. Chesterton Company
 
Superior Impact & Wear Resistant Lining
 
100% solids, impact resistant, ceramic reinforced, epoxy/urethane hybrid lining for severe abrasive wear and impact resistance.
 

 
Mitsubishi Gas Chemical America
 
Performance Amine 1,3-BAC
 
A highly reactive cycloaliphatic diamine offering superior performance. Reasonable cost and curing efficacy makes it suitable for all types of epoxy resin applications.
 

 
HoldTight Solutions Inc.
 
NO FLASH RUST - NO CONTAMINANTS
 
Our HoldTight®102 salt remover & flash rust
preventer prevents flash
rust by removing surface contaminants. Contact us
for your nearest distributor.
(800) 319.8802 sales@holdtight.com
 

 
Vector Technologies Ltd.
 
The Original Performance Proven Vacuum Solutions
 
VecLoader® 616 Double Dump, Continuous Vacuum, 170 HP w/ 2,400 CFM & 28” Hg. 33% More Efficient than traditional vacuum systems! Choose Vector for the most powerful and the most reliable trailer mounted vacuums in the industry! Email us at: inquiry@vector-vacuums.com or call us at: 800-832-4010
 

 
Detail Masters
 
Overspray Removal
 
We offer professional, turnkey service and unparalleled quality!
Our process can save hundreds— even thousands of dollars. It's fast, environmentally safe and 100% guaranteed.
 

 
 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

Durability + Design PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy policy (Updated 1/8/2018)   |   Terms & conditions   |   Site Map   |   Search   |   Contact Us