Improving Polyurethane Pipe Coatings for Harsh Conditions

by Andreas aus der Wieschen, Matthias Wintermantel, Todd Williams and Ahren Olson, Bayer MaterialScience AG

This article describes polyurethane pipe coatings as a versatile product class that can be tailored to meet a wide range of end-use applications by varying the formulation.


Reinforced Storage Tank Linings: Advantages and Applications

by Matthew Fletcher, International Paint Ltd.

The author explains the benefits of using different types of reinforced lining systems to mitigate underside corrosion in steel chemical storage tanks.


In-Shop to Offshore: Shop Coating Steel for the Thornton Bank Wind Farm

by Ronny Van Poppel, Smulders Group

This article describes the shop coating processes used to coat steel jacket parts for the Thornton Bank offshore wind farm. The project received the E. Crone Knoy Award at the SSPC 2014 Structure Awards.


Plus...


Top of the News

Two new, free webinars available


The Buzz


Problem Solving Forum

On coating a stained concrete floor

I need to coat a bare concrete warehouse floor that has visible oil stains. What are my options for cleaning the concrete before coating it?


SSPC Protective Coatings Specialist

Q&A with Patrick Ricciardi, Pacific Titan

by Charles Lange, JPCL


Applicator Training Bulletin

Setting up air abrasive blast equipment


F-Files: Mechanisms of Failure

The case of improperly cleaned surfaces

by Jayson L. Helsel, P.E., KTA-Tator, Inc. Rich Burgess, PCS, KTA-Tator, Inc., Series Editor

Failures in Preparation or Specification?


News

Product News

NLB waterjet boosts safety with distance


Project Preview

Monoko, LLC Awarded O’Neal Bridge Rehab Contract

by Katelyn Antolik, Paint BidTracker


Editorial

Mentorship

by Bill Shoup, Executive Director, SSPC


SSPC News

King starts term as SSPC president; Ackx, Castle re-elected to Board


   
Advertisements
 
Mitsubishi Gas Chemical America
 
Performance Amine 1,3-BAC
 
A highly reactive cycloaliphatic diamine offering superior performance. Reasonable cost and curing efficacy makes it suitable for all types of epoxy resin applications.
 

 
Carboline Company
 
New product: Carbozinc® 608 HB
 
Introducing a new high build zinc-rich primer that can save you time and money by eliminating the epoxy intermediate coat!
 

 
CHLOR*RID International Inc.
 
SOLUTIONS THAT WORK
 
Companies that invest in corrosion control use CHLOR RID products
  • Soluble salt removal liquid
  • Test kits to verify contamination levels
  • Surface passivation to hold the blast
INFO@CHLOR-RID.COM 800.422.3217
 

 
SABRE Autonomous Solutions
 
Safety
 
Removing blasting operators from harmful environments is our key objective.
 

 
Graco Inc.
 
Graco EcoQuip 2: Experience the Difference
 
While others claim their equipment is the same, none of them compare to Graco’s EcoQuip 2™ Vapor Abrasive® blasting line. Visit graco.com/ecoquip to learn more.
 

 
Industrial Vacuum Equipment Corp.
 
Hurricane Vacuums
& Dust Collectors
 
Vacuum and dust collector hose, filters and related accessories.
IndustrialVacuum.com
 

 
Jotun Paints Inc.
 
Jotun Jotachar 1709
 
Mesh-free passive fire protection epoxy designed to protect against hydrocarbon pool fire scenarios for up to four hours as defined in the ANSI/UL1709 standard.
 

 
Tarps manufacturing, Inc.
 
QUALITY MADE IN AMERICA —Available near you!
 
CLICK to get a behind-the-scenes look at how Tarps Manufacturing makes the highest-quality tarps right here in the USA — available nationwide.
 

 
SAFE Systems, Inc.
 
Enduroguard -
The Tough Cable
for a Tough Industry.
 
Reduce maintenance costs and down time, increase job site safety with Enduroguard Cable. Available exclusively from SAFE Systems. UL listed, flexible, abrasion resistant and cut resistant.
 

 
Fischer Technology Inc.
 
FISCHER Expands Corrosion Product Line
 
Rounding out Fischer’s extensive line of products for measuring protective coatings in the corrosion industry is the new ultrasonic wall thickness gauge UMP series.
 

 
 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

Durability + Design PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy policy   |   Terms & conditions   |   Site Map   |   Search   |   Contact Us