Proof positive: ASTM E 2357 standard provides method to measure air-barrier performance

by Mark Kennedy and Craig Boucher, Grace Construction Products

The recently adopted standard test method ASTM E 2357 provides a uniform methodology for testing and measuring the leakage rate of air-barrier assemblies.


Plus...


News

Air-barrier product gets 'Renovation Nation' air time


Contributors


Getting less grief from your EIFS

by Brent Fisher and Bob Dazel, Dryvit Systems Inc.

All exterior cladding systems require routine, consistent maintenance programs to ensure long-term, optimal building performance. EIF systems are no different.


Making it clear on water repellents (Part 1)

by David W. Boyer, PROSOCO Inc.

This two-part examination of clear water repellents for above-grade concrete and masonry includes a review of the various chemistries and compositions, factors that determine their selection, environmental considerations, and application recommendations.


Projects

Powerful medicine

by Joe Maty, Editor, JAC

The architects of the new Pittsburgh Children's Hospital employed vibrant colors, bold design, and attention to sustainable-design priorities in creating a dynamic healing environment.


Product Pipeline

by Technology Publishing


Separating fact from fiction: Myth vs. reality in the mysterious world of mold

by Bryan Redler, EnviroCare Corp.

Presented are five of the most common myths about mold, the hard facts that debunk these myths, and measures that can be taken to prevent mold problems, from design stage forward.


Special Advertising Section

Special Advertising Section: Concrete Polishing

by Technology Publishing

Concrete polishing: Durability, sustainability, creativity.


Passing the Test

Taking cool to the next level

by Allen Zielnik, Atlas Materials Testing Technology

Heat-deflecting technologies aren't relegated to the roof, as coatings makers, users look to capitalize on new applications.


Editor's Word

The air-barrier express hits a curve, but rolls on

by Joe Maty, Editor, JAC

Due to an error in production, the Editor's Word column on page 2 of the August-September issue of JAC was repeated from the June-July issue. The correct August-September Editor's Word is included in the digital edition of this issue. JAC regrets the error.


   

Corrosion Probe, Inc.
From Detection to Correction

Corrosion Probe, Inc. has the Most Concrete Coatings Experience and Expertise. Contact us today at
860-767-4402, www.cpiengineering.com


Dampney Co., Inc.
Rubber In a can!

Rubberized Spray in a
Handy Aerosol Can

• Stays flexible
• Seals off moisture penetration
• Non sagging formulation
• Will not crack, chip or peel
• Apply to wet and dry surfaces
• Paintable


DeFelsko Corporation
NEW PosiTector
Inspection Kits

PosiTector 6000 Coating Thickness Gage easily converts to a surface profile gage, dew point meter or ultrasonic wall thickness gage with a simple probe change.


EDCO - Equipment Development Co. Inc.
EDCO's Quick Response Codes

EDCO now includes Quick Response Code decals on machines. These QRC's provide customers with instant jobsite advice, problem solving tips and much more. Click to watch EDCO machines in action.


Versaflex Inc.
Best NSF 61.5 Approved Potable Water Polyurea

VersaFlex Polyurea Earns Highest ANSI/NSF 61.5 Rating for High Temp Service, Minimum Tank Size and Max Thickness. All Polyureas Are Not Created Equal. FREE WHITE PAPER.


LS Industries
LS Blasters: Optimum Steel Cleaning Efficiency

Simplify surface prep with the precise shot control of LS Blasters. Our blast technology delivers optimum coverage and finish. 800-533-8008


Cardolite Corporation
CNSL Based Products

Renewable CNSL epoxy curing agents and resins with fast cure at low temperature, adhesion to unprepared surfaces and excellent corrosion and water protection.

 
 
 
 
Technology Publishing

The Technology Publishing Network

The Journal of Protective Coatings & Linings (JPCL) PaintSquare
Durability + Design Paint BidTracker JPCL Europe

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy policy   |   Terms & conditions   |   Site Map   |   Search   |   Contact Us
 

© Copyright 2000-2013, Technology Publishing / PaintSquare, All rights reserved
2100 Wharton Street, Suite 310, Pittsburgh PA 15203-1951; Tel 1-412-431-8300; Fax 1-412-431-5428; E-mail webmaster@paintsquare.com